TB0330 is a 2-part liquid silicone with high transparency, great tear-strength and strong bonding force.
Specification:
-Low shrinkage(<0.1%)
-Good skid-proof effect and high adhesive strength
-Wearproof, wash-resistant, high temperature resistant
-Non-toxic and odorless, food grade silicone
-High transparency and good tear-strength.
Application:
It is specially used for skid-proof purpose of frilals, underclothes and widely applied for cotton fabric, polyester-mixed cotton cloth, nylon cloth, flax, woolen, insulating cloth, etc.
Datasheet:
ModelTB0330
AppearanceTransparent
Hardness(shore A)30± 2
Mix ratio(A: B)1: 1
Viscosity(mPa. S)60000~100000
Tensile strength(Mpa)4.6
Tear-strength(KN/m)19± 2
Elongation(%)360
Pot life/working time(25)12-24 hours
Curing time(100-120)10~20(mins)
Operation introduction:
1, Mix Part A and Part B as ratio 1: 1, you may add additive such as pigment as ratio 1~2% into part A.
2, It can be cured by heating with 100~150 degree, the curing time will be 5~10 minutes.
Specification:
-Low shrinkage(<0.1%)
-Good skid-proof effect and high adhesive strength
-Wearproof, wash-resistant, high temperature resistant
-Non-toxic and odorless, food grade silicone
-High transparency and good tear-strength.
Application:
It is specially used for skid-proof purpose of frilals, underclothes and widely applied for cotton fabric, polyester-mixed cotton cloth, nylon cloth, flax, woolen, insulating cloth, etc.
Datasheet:
ModelTB0330
AppearanceTransparent
Hardness(shore A)30± 2
Mix ratio(A: B)1: 1
Viscosity(mPa. S)60000~100000
Tensile strength(Mpa)4.6
Tear-strength(KN/m)19± 2
Elongation(%)360
Pot life/working time(25)12-24 hours
Curing time(100-120)10~20(mins)
Operation introduction:
1, Mix Part A and Part B as ratio 1: 1, you may add additive such as pigment as ratio 1~2% into part A.
2, It can be cured by heating with 100~150 degree, the curing time will be 5~10 minutes.